Effects of CO2 and H2S on corrosion of martensitic steels in brines at low temperature
(Nace International, 2018)
Corrosion studies were conducted for martensitic carbon steels in 5 wt% NaCl brine solutions at 4°C and 10 MPa (1,450 psi). These studies simulated different subsurface environments relevant to Arctic drilling. Here, two ...
The use of papaver somniferum L. Plant extract as corrosion inhibitor
(Pleiades Publishing, Ltd, 2019)
The corrosion inhibition and adsorption characteristics of the extract obtained from the plant Papaver somniferum L. (PSL) by electrochemical methods at different temperatures (25, 35 and 45°C) were investigated in 0.2 M ...
Tertiary amine methacrylate based polymers as Corrosion Inhibitors in double distilled water. Part I
(Pleiades Publishing, Ltd, 2019)
In the current study, the inhibitive performances of tertiary amine methacrlate based water soluble diblock copolymers on the corrosion behaviour of AISI 304 stainless steel were investigated in double distilled water (DDW, ...
Effects of H2S and CO2 on Cement/Casing interface corrosion integrity for cold climate oil and gas well applications
(The Electrochemical Society, 2016)
Low-temperature corrosion relevant to oil and gas wells was investigated. Casing cement was exposed to brine in contact with CO2 at 4 °C and 10 MPa. Pore water was extracted from wet cement using a die press, and a cement ...
Tertiary amine methacrylate based polymers as corrosion ınhibitors in hcl solution. Part II
(Pleiades Publishing, Ltd, 2019)
In this study, the inhibitive performance of novel synthesised water-soluble of different molecular weight diblock copolymers of derivative methyl methacrylate (VB84, VB206, VB207, VB361, VB371,VB406) on the corrosion ...
Investigation of corrosion and wear behavior of borided AISI P20 steel in micro-wave furnace
(IOP Publishing, 2019)
In this study, the effect of microwave boronizing treatment on the corrosion and wear behaviour of boride layer formed on AISI P20 steel have been investigated. The boronizing treatment was carried out using Ekabor-II ...
Electrochemical corrosion behavior of high velocity Oxy-Fuel (HVOF) superalloy coatings on ductile irons
(Sakarya University Journal of Science, 2019)
In this study, alloyed and unalloyed ductile irons (DI) were coated with two different Ni-based superalloy materials by HVOF method. Microstructure and phase analyzes of the coatings were performed by using SEM, EDX, XRD ...
Formation of deposit and corrosion in Afyonkarahisar geothermal heating system [Afyonkarahisar jeotermal isitma sisteminde oluşan kabuklaşma ve korozyon]
(TMMOB jeoloji müdendisleri odası, 2008)
The formation of deposit and corrosion, which was formed depending on the chemical composition of the geothermal water, is one of the most serious problems at the geothermal systems. In this study, ion chromotography (IC) ...
Hydroxyapatite (HAP) coating with biomimetic method abstract
(Afyon Kocatepe Üniversitesi, 2009)
Biomimetik yöntemle hidroksiapatit (HAP) kaplama en gelecek vaat eden tekniklerden birisidir. Bu çalışmada, üç farklı ön yüzey işlemi (HNO3, anodik polarizasyon, 5 N NaOH-1 N HCl (BA)) altlıkların (Ti ve Ti6Al4V) yüzey ...
Corrosion behavior of boro-tempered ductile iron
(Springer, May 2010)
In this study, the effect of boro-tempering heat treatment on the microstructure and corrosion behavior of unalloyed ductile iron was investigated. The corrosion characteristics of ductile iron have been determined by ...