dc.identifier.citationJustin Beck, Ruishu Feng, Derek M. Hall, Aysel Buyuksagis, Serguei N. Lvov, Margaret Ziomek-Moroz, “Corrosion of 13Cr Steel at the Cement/Casing Interface in CO2/H2S Environments at 4, 85 and 200 °C”, NACE CORROSION 2018, April 15-19, Phoenix, Arizona, Paper No: 11015en_US
dc.identifier.urihttp://nacecorrosion.org/
dc.identifier.urihttps://hdl.handle.net/11630/7592
dc.description.abstractA study was carried out to investigate corrosion at the cement/casing interface for 13Cr casing steel. Cement simulated pore solution (CSPS) was developed by exposing cement pieces to 5% NaCl at 100 °C and 10 MPa in equilibrium with CO2. Pore solution was extracted from the cement pieces using a die press. Chemical analysis of the pore solution extract was performed and used for preparing CSPS for 13Cr corrosion testing. Corrosion tests were performed in CSPS at equilibrium with CO2 or CO2+H2S at 10 MPa at 4, 85, and 200 °C. Corrosion rates were determined using linear polarization resistance (LPR), electrochemical impedance spectroscopy (EIS), and mass loss coupons. Addition of H2S at 4 °C increased the corrosion rate, while at 85 °C it slightly decreased the corrosion rate. Only a small effect from H2S addition was observed at 200 °C. Cyclic voltammetry (CV) results showed passivation/depassivation of 13Cr in CSPS at 4 and 85 °C, while a transition to active corrosion was observed at 200 °C. Surface analysis using scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS) found that both the coverage and complexity of the corrosion products formed increased dramatically with increasing temperature.en_US
dc.language.isoengen_US
dc.publisherNace Internationalen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectH2S Corrosionen_US
dc.subjectCO2 Corrosionen_US
dc.subjectChromium Steelsen_US
dc.subjectCorrosion Ratesen_US
dc.subjectCorrosion Productsen_US
dc.subjectCold Climate Conditionsen_US
dc.subjectHigh Pressureen_US
dc.subjectHigh Temperatureen_US
dc.titleCorrosion of 13Cr steel at the Cement/Casing interface in CO2/H2S environments at 4, 85 and 200 °Cen_US
dc.typeconferenceObjecten_US
dc.relation.journalNACE İnternational CORROSION 2018en_US
dc.departmentFen-Edebiyat Fakültesien_US
dc.authorid0000-0001-8911-7157en_US
dc.identifier.startpage11015en_US
dc.relation.publicationcategoryKonferans Öğesi - Uluslararası - Kurum Öğretim Elemanıen_US
dc.contributor.institutionauthorBüyüksağiş, Aysel


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster