Tertiary amine methacrylate based polymers as corrosion ınhibitors in hcl solution. Part II
(Pleiades Publishing, Ltd, 2019)
In this study, the inhibitive performance of novel synthesised water-soluble of different molecular weight diblock copolymers of derivative methyl methacrylate (VB84, VB206, VB207, VB361, VB371,VB406) on the corrosion ...
Corrosion behaviors of hydroxyapatite coated by electrodeposition method of Ti6Al4V, Ti and AISI 316L SS substrates
(Pleiades Publishing, Ltd, 2013)
Electrodeposition method was used to obtain hydroxyapatite (HAP) coatings on Ti6Al4V, Ti and AISI 316L SS substrates. Electrodeposition solution is prepared as Ca(NO3)2 ⋅ 4H2O and (NH4)H2PO4. Additionally, three different ...
The examination of Afyonkarahisar's geothermal system corrosion
(ASM International, 2013)
Corrosion and scaling of metal surfaces are the major problems caused by geothermal fluids when metallic structures are used. This article describes a study of corrosion and scaling problems in the Afyonkarahisar Geothermal ...
Electrochemical corrosion of Ti6Al4V, Ti and AISI 316L SS after immersed in concentrated simulated body fluid
(Pleiades Publishing, Ltd, 2016)
The biomimetic method is used to obtain hydroxyapatite (HAP) coatings on Ti6Al4V, Ti and AISI 316L SS substrates. These substrates with different pretreatment surface operations (HNO3, anodic polarization, base-acid) were ...
Tertiary amine methacrylate based polymers as Corrosion Inhibitors in double distilled water. Part I
(Pleiades Publishing, Ltd, 2019)
In the current study, the inhibitive performances of tertiary amine methacrlate based water soluble diblock copolymers on the corrosion behaviour of AISI 304 stainless steel were investigated in double distilled water (DDW, ...
Corrosion inhibition of st37 steel in geothermal fluid by quercus robur and pomegranate peels extracts
(Pleiades Publishing, Ltd, 2015)
Plant extracts have become important as an environmentally acceptable, readily available and renewable source of wide range of inhibitors. Tannins, a class of natural, non toxic and biodegradable polyphenolic compounds, ...
Corrosion and wear behaviors of boronized AISI 316L stainless steel
(Springer, 2013)
In this study, the effects of a boronizing treatment on the corrosion and wear behaviors of AISI 316L austenitic stainless steel (AISI 316L) were examined. The corrosion behavior of the boronized samples was studied via ...
Corrosion behaviour of coatings on 304 steel
(ASIAN PUBLICATION CORPORATION, 2012)
The aim of this study is to determine the corrosion characteristics of 304 steel by the methods of Tafel extrapolation, linear polarization and electrochemical impedance spectroscopy (EIS). The steel surface is covered ...
Investigation of corrosion behavior of borided gear steels
(Springer, 2014)
In this study, corrosion behaviors of GS18NiMoCr36 (GS 18) and GS32NiCrMo6.4 (GS 32) gear steels borided in Ekabor-II powder at the temperature of 950 °C for 2 and 6 h were investigated in a 6 % M HCI acid solution. The ...