dc.contributor.author | Gültekin, Deniz | |
dc.date.accessioned | 2021-08-02T07:36:06Z | |
dc.date.available | 2021-08-02T07:36:06Z | |
dc.date.issued | 24.02.2021 | en_US |
dc.identifier.citation | Gültekin, D . (2021). Akımsız Kaplama Yöntemi ile CeO2 Takviyeli Ni-B Nanokompozit Kaplama Üretimi ve Karakterizasyonu . Afyon Kocatepe Üniversitesi Fen Ve Mühendislik Bilimleri Dergisi , 21 (1) , 209-216 . DOI: 10.35414/akufemubid.820183 | en_US |
dc.identifier.uri | https://dergipark.org.tr/tr/pub/akufemubid/issue/60443/820183 | |
dc.identifier.uri | https://doi.org/10.35414/akufemubid.820183 | |
dc.identifier.uri | https://hdl.handle.net/11630/8974 | |
dc.description.abstract | Ni-B ve Ni-B-CeO2 nanokompozit kaplamalar nikel sülfat hekzahidrat, dimetilamin boran, sodyum asetat ve tiyoüre içeren kaplama banyosu kullanılarak akımsız kaplama işlemi ile üretilmiştir. Nanokompozit üretiminde kullanılan CeO2 nanopartikül takviyelerinin boyutu 100-500 nm aralığındadır. Takviye partiküllerinin banyo içerisinde kolay dağılımını ve ıslanabilirliğini artırmak için sodyum dodesil sülfat kullanılmıştır. Takviye partikül miktarı 15 gr/lt olarak seçilmiştir. Saf Ni-B ve nanokompozit Ni-B-CeO2 akımsız kaplamalar için banyo pH değeri 6, kaplama süresi 60 dakika ve banyo sıcaklığı 70 °C ± 5 °C olarak belirlenmiştir. Takviye CeO2 nanopartiküllerinin kaplamanın morfolojisi ve sertliği üzerindeki etkileri incelenmiştir. Yapılan karakterizasyon işlemleri sonucunda nanoboyutlu CeO2 partiküllerinin Ni-B alaşımına başarılı bir şekilde ilave edildiği ve nanokompozit kaplama üretiminin gerçekleştirildiği belirlenmiştir. Bununla birlikte takviye malzemenin etkisinin karşılaştırmalı olarak incelenmesi amacıyla aynı banyo bileşimi kullanılarak takviyesiz saf Ni-B kaplama da üretilmiştir. CeO2 nanopartiküllerinin Ni-B matrisine ilave edilmesiyle hesaplanan Ni kristal boyutu 43 nm'den 24,9 nm'ye düşmüştür. Ayrıca saf Ni-B alaşımı ile kıyaslandığında CeO2 takviyeli Ni-B nanokompozit kaplamanın sertlik değerinde de artış meydana geldiği belirlenmiştir. | en_US |
dc.description.abstract | Ni-B and Ni-B-CeO2 nanocomposite coatings were produced by electroless coating process using a coating bath containing nickel sulphate hexahydrate, dimethylamine borane, sodium acetate and thiourea. The size of the CeO2 nanoparticle reinforcements used in nanocomposite production is in the range of 100-500 nm. Sodium dodecyl sulfate was used to increase the easy dispersion and wettability of the reinforcement particles in the bath. The amount of reinforcement particles is determined as 15 g/lt. For pure Ni-B and nanocomposite Ni-B-CeO2 electroless coatings, bath pH value was 6, coating time was 60 minutes and bath temperature was 70 °C ± 5 °C. The effects of CeO2 particles used as reinforcement on the morphology and hardness of coating were investigated. Nano-sized CeO2 particles were successfully incorporated into the Ni-B alloy and nanocomposite coating was produced. Also, Ni-B coating without reinforcement was produced using the same bath composition in order to compare the effect of the reinforcement material. Due to the incorporation of CeO2 nanoparticles in the Ni-B matrix, the calculated Ni crystal size decreased from 43 nm to 24.91 nm. In addition, it was determined that the hardness of the CeO2 reinforced Ni-B nanocomposite coating increased when compared to the pure Ni-B alloy. | en_US |
dc.language.iso | tur | en_US |
dc.publisher | Afyon Kocatepe Üniversitesi | en_US |
dc.identifier.doi | 10.35414/akufemubid.820183 | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Akımsız Kaplama | en_US |
dc.subject | Nanokompozit | en_US |
dc.subject | Ni-B | en_US |
dc.subject | CeO2 | en_US |
dc.subject | Electroless Coating | en_US |
dc.subject | Nanocomposite | en_US |
dc.subject | Ni-B | en_US |
dc.subject | CeO2 | en_US |
dc.title | Akımsız kaplama yöntemi ile CeO2 takviyeli Ni-B nanokompozit kaplama üretimi ve karakterizasyonu | en_US |
dc.title.alternative | CeO2 reinforced Ni-B nanocomposite coating production and characterization by electroless coating method | en_US |
dc.type | article | en_US |
dc.relation.journal | Afyon Kocatepe Üniversitesi Fen ve Mühendislik Bilimleri Dergisi | en_US |
dc.department | Fakülteler, Teknoloji Fakültesi, Metalurji ve Malzeme Mühendisliği Bölümü | en_US |
dc.authorid | 0000-0002-6941-7539 | en_US |
dc.identifier.volume | 21 | en_US |
dc.identifier.startpage | 209 | en_US |
dc.identifier.endpage | 216 | en_US |
dc.identifier.issue | 1 | en_US |
dc.relation.publicationcategory | Makale - Ulusal Hakemli Dergi - Başka Kurum Yazarı | en_US |